Gold Refinery NYC

Gold Assay in NYC: What Each Test Tells You

A crucible crusted with gold residue and a steel ladle at a foundry

An assay answers one question: how much precious metal is really in this? Every fair price for gold, silver or platinum rests on that answer, so it is worth knowing how it is reached. The word sounds old because it is. Assayers have been testing gold for as long as people have traded it, and some of the methods we use at 30 West 47th Street would be familiar to an assayer from centuries ago. Others read the metal with X-rays in a few minutes.

We assay gold, silver and platinum as part of refining and buying. This page explains the methods, what each one is good at, and what each can miss.

Need to know what your metal really is? Call or send the form.

Assay methods compared

There is no single correct test. Each method trades speed and convenience against precision and whether the piece survives. The accuracy figures here are the typical ranges given in reference sources for each method, not a promise about any one test.

MethodDestroys the piece?Typical precisionSpeedSuits
Touchstone and acidNo, a small streak on the stoneAbout 10 to 20 parts per thousandMinutesSingle pieces of jewelry, a quick karat check
XRF on the pieceNoAbout 2 to 5 parts per thousandAbout three minutesFlat, larger surfaces; jewelry, coins, bars
Melt, sample, then XRFYes, the lot is melted into one barReads the whole lot, not just the surfaceLonger: the melt comes firstMixed scrap, dental gold, anything plated or soldered
Fire assay (cupellation)Yes, a small sample is consumedDown to about 1 part in 10,000 on bullionThe slowestBullion, large lots, settling a disagreement

The touchstone and acid test

The oldest method still in daily use. The piece is rubbed on a dark stone, leaving a thin streak of metal. Acids of known strength go on the streak, and the result is compared with streaks from test needles of known karat. If 14 karat acid dissolves the streak, the metal is below 14 karat. A skilled tester can tell karats apart quickly, and the piece itself is unharmed.

The limits: the acid only sees the surface the stone touched, so a heavy plating over base metal can fool a careless test, and the precision is coarse compared with instruments.

X-ray fluorescence

XRF shines X-rays at the metal and reads the energy given back, which is different for each element. In about three minutes it reports gold, silver, copper, zinc, palladium and more, without a mark on the piece. It works well on flat, reasonably large surfaces such as bars, coins and the backs of pendants.

The limit is that XRF reads the surface. On a plated piece it reads the plating. On a hollow or filled piece it cannot see inside. That is why, for lots where the surface may not match the inside, we melt first.

Melting and sampling

When you bring a mixed lot, testing each piece is slow and still leaves solder, springs and clasps unaccounted for. Melting the whole lot into one bar mixes everything evenly. A sample taken from the center of the melt then represents the whole lot, and it can be read by XRF or fire assayed. For dental gold and sweeps this is the only fair way to work.

Fire assay

Fire assay, also called cupellation, is the most exact method and the accepted standard for bullion at major refineries. A small, carefully weighed sample is wrapped with lead and heated in a cupel, a porous cup that soaks up the lead and the base metals with it. What is left is a bead of gold and silver. The silver is dissolved in acid, and the gold that remains is weighed. Done on bullion to international standards, the method can be accurate to about one part in ten thousand.

The cost is time and a small amount of metal. Fire assay makes sense for bullion, for large lots where a fraction of a percent is real money, and whenever two parties want a figure neither can argue with.

Which test for which metal

  • A ring, chain or pendant with a clear stamp: acid or XRF, piece left whole.
  • A bag of mixed karat jewelry: sort by stamp and test, or melt and sample.
  • Dental gold: melt and assay; the alloys vary too much to guess.
  • Filings and sweeps: processed first, then melted and assayed.
  • A bar or coin: XRF to confirm the mark; fire assay for a large or unmarked bar.
  • Sterling or coin silver: XRF or melt and sample; see our silver refinery page.
  • Platinum and palladium jewelry: XRF reads them well; marks such as 950 Pt are a guide.

What the stamp says, and what the law allows

A 14K stamp is the maker’s claim. Under the National Stamping Act, gold articles without solder may assay up to three parts per thousand under their mark, and up to seven parts per thousand when the part tested contains solder. Sterling has a tolerance of four parts per thousand without solder. Pieces made abroad, very old pieces and repaired pieces can be well outside those ranges, which is the whole reason for testing.

Why two tests can disagree

It is common for a piece to read one figure on an acid test and a slightly different one on XRF. Neither is wrong. The acid sees a streak from one spot; XRF averages a small area of the surface; a melt sample sees the whole alloy. On a solid, well made piece the figures land close together. Where they differ, the difference itself tells us something, usually that there is solder, a repair or a plating somewhere. When the stakes justify it, the melt and a fire assay settle the question for good.

If you want a figure you can take elsewhere, ask for the method used to be written down with the result. A fineness without its method is hard to compare.

How the assay turns into a number

Once the fineness is known, the price follows: troy weight times fineness times spot, less the refining charge. Our sell gold in NYC page works that through with real karat figures, and the live gold prices page shows the day’s spot.

Common questions

What is a gold assay?

A test that measures how much gold, silver or other metal is in a piece or a lot, usually given in parts per thousand.

Where can I get gold assayed in NYC?

On West 47th Street. We assay gold, silver and platinum at 30 West 47th Street, 8th Floor.

Does an assay damage my jewelry?

Acid and XRF leave the piece whole. Fire assay and melt sampling use up metal, so they suit scrap, lots and bullion.

Which gold test is the most accurate?

Fire assay. On bullion it can reach about one part in ten thousand.

Can XRF be fooled by plating?

It reads the surface, so a thick plating can mislead it. Melting and sampling avoids that.

Why does my 14K piece test lower?

Solder, springs, repairs and older or foreign manufacture all pull the real figure under the stamp.

Ask for a refining quote

Tell us what you have and we will call you back.

Sending this costs nothing and commits you to nothing. The refinery reads your request and replies by phone or email; a firm number comes only after your metal is weighed and assayed.

Call the refinery(212) 704-9703